▎ 摘 要
NOVELTY - Preparation of protective nonwoven fabric involves uniformly mixing p-aminobenzotrifluoride, n-octylamine, alkylaminoglucitol and 4-amino-1,2,4-triazole with dioxane, adding material (C), reacting at 65-75 degrees C for 6-10 hours, reacting, washing, drying, obtaining material (D), adding graphene oxide to water, adjusting pH to alkaline, ultrasonically processing for 2-3 hours, adding glucose, reacting at 65-75 degrees C for 5-8 hours, mixing with hydroxylamine hydrochloride, allicin, zinc complex, lentinan and silk fibroin, adding material (D), carrying out padding treatment and drying. USE - Preparation of protective nonwoven fabric. DETAILED DESCRIPTION - The material (C) is obtained by washing polypropylene composite nonwoven fabric, drying, subjecting to plasma treatment, maintaining in air, obtaining material (A), mixing 1-hydroxy-cyclohexyl-phenyl ketone, fluorinated acrylic resin, octadecyl methacrylate, glycidyl acrylate, lauryl acrylate, fatty alcohol ethoxylate and ethylene glycol dimethacrylate with water, obtaining material (B), adding material (A) to material (B), carrying out ultraviolet light irradiation grafting reaction under protection of nitrogen, washing and drying.