• 专利标题:   Preparing efficient and environmentally friendly steel slag composite activator, comprises uniformly mixing polyol amine, polyol, sodium acetate, graphene, and dihydrate gypsum at room temperature, and mechanically stirring to obtain steel slag composite activator.
  • 专利号:   CN115611546-A
  • 发明人:   YANG C, LIU Y, JIAN X, WANG J, MU C, XING X, YANG X, YIN L
  • 专利权人:   UNIV CHINA YANGTZE DELTA REGION ELECTRON
  • 国际专利分类:   C04B024/12, C04B028/00
  • 专利详细信息:   CN115611546-A 17 Jan 2023 C04B-024/12 202313 Chinese
  • 申请详细信息:   CN115611546-A CN11243780 11 Oct 2022
  • 优先权号:   CN11243780

▎ 摘  要

NOVELTY - Preparing efficient and environmentally friendly steel slag composite activator, comprises uniformly mixing 0.2-0.4 pts. wt. polyol amine, 1-2 pts. wt. polyol, 0.4-0.6 pts. wt. sodium acetate, 0.1-0.3 pts. wt. graphene, and 0.2-0.6 pts. wt. dihydrate gypsum at room temperature, and mechanically stirring for 10 minutes to obtain a steel slag composite activator. USE - The method is useful for preparing efficient and environmentally friendly steel slag composite activator. ADVANTAGE - The steel slag composite excitant can reasonably use large amount of waste steel slag material, after mixing with the cement, improving the activity index and stability. The preparation method is simple and efficient, it is suitable for industrial production, and is good for reducing the use amount of the clinker and discharging carbon dioxide. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for method for using steel slag composite activator.