▎ 摘 要
NOVELTY - Material comprises 20-30 pts. wt. hydrogen-rich water porcelain, 10-15 pts. wt. three-dimensional graphene, 15- 25 pts. wt. anionic powder, 30-40 pts. wt. shell powder, 3-10 pts. wt. binder, 3-6 pts. wt. activated carbon, 2-5 pts. wt. zeolite, 2-6 pts. wt. nano silver carbon molecular sieve, 1-3 pts. wt. titanium dioxide, and 2-3 pts. wt. manganese dioxide nanometer Line. USE - Material used to clean fruits, vegetables, and tableware, and manufacture hydrogen-rich water, health care, and beauty industries (claimed). ADVANTAGE - The material has oil removal and pesticide removal function. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a material, which involves: (A) mixing hydrogen-rich water porcelain, anion powder, shell powder, zeolite and grinding to a powder particle size of less than 100 microns; (B) baking the material, where the baking temperature is 150-350 degrees C, and the baking time is 2-5 hours; (C) sieving the material with a mesh sieve of less than 100 micrometer to obtain a powder; (D) mixing the powder with three-dimensional graphene, activated carbon, nano silver carbon molecular sieve, titanium dioxide, manganese dioxide nanowire; (E) adding the mixed material to a ball forming machine, and continuously spraying the binder during the molding process; and (F) firing the shaped material at 900-1000 degrees C, and then sieving to obtain a material.