• 专利标题:   Electrolyte for organic nickel ion battery, comprises soluble nickel salt and organic ether solvent.
  • 专利号:   CN114204137-A
  • 发明人:   HUANG C, CHEN S, ZHAO Y
  • 专利权人:   SOUTH CHINA COLLABORATIVE INNOVATION INS
  • 国际专利分类:   H01M010/26, H01M010/30, H01M004/58
  • 专利详细信息:   CN114204137-A 18 Mar 2022 H01M-010/26 202244 Chinese
  • 申请详细信息:   CN114204137-A CN11269654 29 Oct 2021
  • 优先权号:   CN11269654

▎ 摘  要

NOVELTY - Electrolyte comprises a soluble nickel salt and an organic ether solvent. USE - Electrolyte of organic nickel ion battery used in portable computer, mobile phone and space flight. Can also be used in lithium ion battery. ADVANTAGE - The electrolyte is capable of actually working, and successfully assembling the organic nickel ion battery. The battery has a voltage window of up to 1.7V, it has good multiplying power performance and cycle performance. Compared with the traditional lithium ion battery, the battery does not have the problem that the electrode material is dissolved in the electrolyte, which greatly improves the service life of the battery. At the same time, the electrode sheet and electrolyte are simple to prepare, and exhibits excellent electrochemical performance, it is expected to become the first-generation secondary battery, it also will enrich the current energy source storage system, and has great application value and prospect. DETAILED DESCRIPTION - INDEPENDENT CLAIMS are included for: 1. An organic nickel ion battery, which comprises an anode, a cathode, a diaphragm and an electrolyte of organic nickel ion battery. 2. An assembling method of the organic nickel ion battery, which involves using titanium foil as current collector, mixing the anode active material, binder and conductive agent uniformly, then dripping N-methyl pyrrolidone diluent, grinding and stirring until forming uniform and stable slurry and uniformly coating on the titanium foil, and then drying to obtain the anode, polishing the cathode material to the surface bright, adding the polished cathode material into absolute ethyl alcohol, ultrasonically drying to obtain the cathode; (3) dissolving the soluble nickel salt in organic ether solvent to obtain electrolyte, then assembling into CR2032 button battery. DESCRIPTION OF DRAWING(S) - The drawing shows a charging and discharging curve diagram of the embodiment 1 of the present invention nickel ion battery in the range of the voltage range 0.1-1.7V current density is 10mA/g. (Drawing includes non-English language text). Diluent (20)