▎ 摘 要
NOVELTY - The preparation method of graphene polymerization modified polyamide 6 high oriented yarn involves melt-spinning the graphite polymerization modified polyamide 6 sections, and cooling to obtain pre-oriented yarn, and drawing, where the spinning speed is 4500-5000 m/minute. USE - Preparation method of graphene polymerization modified polyamide 6 high oriented yarn (claimed). ADVANTAGE - The method enables preparation of graphene polymerization modified polyamide 6 high oriented yarn with stable quality, excellent antistatic performance, 4.32-4.41 dN/dTex tensile strength, and elongation rate of 35-45%.