• 专利标题:   Composite glue comprises component A and B, where component A comprises, where component A comprises epoxy resin, alumina-coated graphite graphene, epoxy silicone coupling agent and dibenzyl phosphate, and has excellent mechanical property.
  • 专利号:   CN107880827-A
  • 发明人:   LI L
  • 专利权人:   HUNAN QIWEI TECHNOLOGY CO LTD
  • 国际专利分类:   C09J163/00, C09J183/10, C09J163/04, C09J011/04, C09J011/06, C08G077/44
  • 专利详细信息:   CN107880827-A 06 Apr 2018 C09J-163/00 201832 Pages: 11 Chinese
  • 申请详细信息:   CN107880827-A CN11110510 12 Nov 2017
  • 优先权号:   CN11110510

▎ 摘  要

NOVELTY - Composite glue comprises component A and B, where component A comprises 45-65 pts. wt. epoxy resin, 10-20 pts. wt. alumina-coated graphite graphene, 5-8 pts. wt. epoxy silicone coupling agent and 5-10 pts. wt. dibenzyl phosphate. The component B comprises 45-65 pts. wt. amino silicone oil, 5-8 pts. wt. aminosilane coupling agent and 10-20 pts. wt. alumina coated graphene. The weight ratio of component A and B is 1:1-2. USE - Composite glue. ADVANTAGE - The composite glue is simple to prepare, and has excellent mechanical, insulating and sealing, waterproof, thermal conductivity, fire resistance, chemical stability and adhesive properties. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing composite glue, which involves: (A) mixing component A and B; (B) stirring the obtained mixture at 70-80/oC; (C) stirring the obtained mixture again for 60-80 minutes, after melting the mixture into liquid state; (D) pouring the mixture on the surface to be coated; (E) standing the obtained product at room temperature for 3-5 hours; (F) drying the obtained product in a drying box at 120-150 degrees C; and (G) keeping the temperature for 4-6 hours, fully solidifying.