• 专利标题:   Preparing anti-glare film material comprises taking oleic acid, polyol, ethyl orthosilicate, and nano-graphene oxide, heating, stirring and reacting, adding ammonia water to adjust the pH, filtering, washing and drying.
  • 专利号:   CN109021553-A
  • 发明人:   WANG M, LAN M, SONG Y
  • 专利权人:   WANG M
  • 国际专利分类:   C08L075/08, C08K013/06, C08K009/12, C08K003/04, C08K003/08, C08K003/22, C08J005/18
  • 专利详细信息:   CN109021553-A 18 Dec 2018 C08L-075/08 201910 Pages: 9 Chinese
  • 申请详细信息:   CN109021553-A CN11135155 28 Sep 2018
  • 优先权号:   CN11135155

▎ 摘  要

NOVELTY - Preparing anti-glare film material comprises (i) taking 20-30 pts. wt. oleic acid, 20-30 pts. wt. polyol,20-30 pts. wt. ethyl orthosilicate, and 5-8 pts. wt. nano-graphene oxide, heating, stirring and reacting, adding ammonia water to adjust the pH to 8.6-8.9, filtering, washing and drying to obtain pre-treated powder, (ii) mixing 20-30 pts. wt. bread worms, 2-3 pts. wt. slag and 10-30 pts. wt. water, mixing juice and fermenting to obtain pretreatment additive, (iii) taking 60-80 pts. wt. aqueous polyurethane emulsion, 15-20 pts. wt. pretreated powder, 10-20 pts. wt. plant essential oil, 10-20 pts. wt. modified additive, 3-5 pts. wt. phospholipid, 2-3 pts. wt. nano metal powder and 2-3 pts. wt. weak oxidant and mixing to obtain anti-glare film material. USE - The method is useful for preparing anti-glare film material. ADVANTAGE - The method produces product has excellent anti-glare property and mechanical property.