▎ 摘 要
NOVELTY - Preparation of asphalt concrete involves heating asphalt to 135-145 degrees C, heat preserving for 15-25 minutes, adding cement, and polyaniline-graphene oxide composite, mixing and stirring at 95-105 rpm for 35-45 minutes, adding strontium-fluorine-doped silver tin oxide, sea squirt cellulose nanocrystals, pretreated blast furnace slag-doped polyacetylene, stirring at 115-125 rpm for 35-45 minutes, obtaining mixture (A), adding the mixture (A) to a reaction kettle, heating to 555-565 degrees C, heat preserving for 55-65 minutes, adding dispersant, sodium polyphosphate, and calcium lignosulfonate in sequence, to a high-speed mixer, and stirring at 185-195 rpm for 35-45 minutes. USE - Preparation of asphalt concrete. ADVANTAGE - The method provides asphalt concrete with excellent electrical conductivity, and conductive performance.