▎ 摘 要
NOVELTY - Heat-absorbing anti-corrosion energy-saving coating comprises 10-30 pts. wt. boron nitride, 20-40 pts. wt. carborundum, 20-40 pts. wt. corundum, 10-20 pts. wt. talc, 5-10 pts. wt. graphene, 10-30 pts. wt. iron oxide red, 10-30 pts. wt. iron oxide black and water glass solvent. USE - Heat-absorbing anti-corrosion energy-saving coating. ADVANTAGE - The product has good heat absorbing effect and strong anti-corrosion function; prolongs service life of the boiler; and is good for heat energy transmission. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of heat-absorbing anti-corrosion energy-saving coating comprising mixing boron nitride, carborundum, corundum, talc, graphene, red iron oxide and black iron oxide in the container, slowly adding 3 times the amount of water glass solvent, adding water glass while stirring, stirring for 4-6 minutes and uniformly mixing.