• 专利标题:   Preparing high-yield fluorinated graphene involves wiehing graphite fluoride and intercalation agent in certain ratio, mixing graphite fluoride and intercalation agent, sealing in built-in container, and placing container.
  • 专利号:   CN107399734-A
  • 发明人:   CHEN J, LIU J, MA H, LI Q, LV Z, WU J, ZHANG L
  • 专利权人:   FUJIAN MENGSHI NEW ENERGY TECHNOLOGY CO
  • 国际专利分类:   C01B032/184, C01B032/194
  • 专利详细信息:   CN107399734-A 28 Nov 2017 C01B-032/184 201801 Pages: 7 Chinese
  • 申请详细信息:   CN107399734-A CN10675774 09 Aug 2017
  • 优先权号:   CN10675774

▎ 摘  要

NOVELTY - Preparing high-yield fluorinated graphene involves wiehing graphite fluoride and intercalation agent in ratio of 1:(0.1-1), mixing graphite fluoride and intercalation agent, sealing in a built-in container, placing sealed container in a reaction vessel, sealing reactor, and reactor evacuating. The liquefying carbon dioxide is injected into the reactor, reached supercritical state of carbon dioxide, holded pressure, reduced pressure so that the pressure in the reactor drops to atmospheric pressure. USE - Method for preparing high-yield fluorinated graphene (claimed). ADVANTAGE - The method enables to prepare high-yield fluorinated graphene in simple and cost-effective manner, which has high yield, high regularity, and has high quality. DETAILED DESCRIPTION - Preparing high-yield fluorinated graphene involves wiehing graphite fluoride and intercalation agent in ratio of 1:(0.1-1), mixing graphite fluoride and intercalation agent, sealing in a built-in container, placing sealed container in a reaction vessel, sealing reactor, and reactor evacuating. The liquefying carbon dioxide is injected into the reactor, reached supercritical state of carbon dioxide, holded pressure, reduced pressure so that the pressure in the reactor drops to atmospheric pressure. The supercritical carbon dioxide is subjected into the circulating flow state, the intercalation agent is gradually extracted, followed by constant temperature cycle dynamic holding pressure, and then down to atmospheric pressure, repeated for 2-5 times. The intercalation agent is added in the reaction vessel which is extracted, built-in vessel is taken out to obtain final product.