▎ 摘 要
NOVELTY - A far-infrared anion magnetic therapy mat preparing method involves thoroughly mixing 50-100 pts. wt. anion additive, 0-50 pts. wt. graphene powder, 0-50 pts. wt. bamboo charcoal, 0-30 pts. wt. adhesive and 5-10 pts. wt. water to prepare paste slurry. The molding method is utilized to step on the woven cloth or the non-woven fabric to adhere the appropriate amount of the slurry to the surface of the cloth using a special abrasive tool, followed by flatly adhering the cloth of the same size to the woven or non-woven fabric to form a three-layered structure of cloth, slurry and cloth in turn, adding a layer of rayon to increase the comfort, sewing the layers with a thread, stitching with a straight line, taking both vertical and horizontal directions, washing with water and removing the adhesive in the slurry to obtain the finished product. USE - Method for preparing far infrared anion magnetic therapy mat.