• 专利标题:   Preparing hyaluronic acid/graphene oxide nanocomposite hydrogel used to control drug release comprises dissolving tyramine grafted hyaluronic acid in graphene oxide phosphate buffered saline solution, reacting with e.g. hydrogen peroxide.
  • 专利号:   CN103980505-A, CN103980505-B
  • 发明人:   CAO Z, LIAO L, SONG F
  • 专利权人:   UNIV WUHAN
  • 国际专利分类:   A61K031/337, A61K031/352, A61K038/47, A61K047/04, A61K047/36, A61K009/06, A61L027/44, A61L027/58, C08B037/08, C08J003/075, C08K003/04, C08K009/00, C08L005/08
  • 专利详细信息:   CN103980505-A 13 Aug 2014 C08J-003/075 201510 Pages: 7 Chinese
  • 申请详细信息:   CN103980505-A CN10226869 27 May 2014
  • 优先权号:   CN10226869

▎ 摘  要

NOVELTY - Preparing hyaluronic acid/graphene oxide nanocomposite hydrogel comprises preparing tyramine grafted hyaluronic acid by adding hyaluronic acid into 2-(N-morpholino)ethanesulfonic acid buffer solution, mixing uniformly, adding ethyl(dimethylaminopropyl) carbodiimide (EDC) and N-hydroxysuccinimide (NHS), stirring, adding tyramine, reacting, dialyzing, freeze-drying, dissolving in phosphate buffered saline (PBS) solution of graphene oxide, adding horseradish peroxidase (HRP) and hydrogen peroxide, quickly stirring, allowing to stand at 20-40 degrees C, and reacting for 30 minutes to 1 hour. USE - The hydrogel is useful for controlling drug release. ADVANTAGE - The method is simple and easy; and has mild reaction conditions. The hydrogel has high mechanical properties and biocompatibility; controls drug release; and has different drug release behavior based on different pH including fast release at high pH and slow release at low pH. DETAILED DESCRIPTION - Preparing hyaluronic acid/graphene oxide nanocomposite hydrogel comprises (a) preparing tyramine grafted hyaluronic acid by adding hyaluronic acid into 2-(N-morpholino)ethanesulfonic acid buffer solution, mixing uniformly, adding ethyl(dimethylaminopropyl) carbodiimide (EDC) and N-hydroxysuccinimide (NHS), stirring for 30 minutes to 1 hour, adding tyramine, reacting at 20-60 degrees C for 10-24 hours, dialyzing for 2-6 days, and freeze-drying, and (b) dissolving in phosphate buffered saline (PBS) solution of graphene oxide to obtain a mixed solution, adding horseradish peroxidase (HRP) and hydrogen peroxide, quickly stirring, allowing to stand at 20-40 degrees C, and reacting for 30 minutes to 1 hour. An INDEPENDENT CLAIM is also included for hyaluronic acid/graphene oxide nanocomposite hydrogel medicinal composition, comprising a drug including rhodamine B, paclitaxel and lysozyme.