▎ 摘 要
NOVELTY - The method involves coating a flexible substrate with glue. The flexible substrate is attached with graphene of a raw substrate. The glue coated flexible substrate is heated at temperature of 90-120 degree Celsius for 30-120 minutes. The flexible substrate is bonded with a hard substrate at light room temperature. The hard substrate is filled with corrosive liquid. A graphene substrate or the flexible substrate and the hard substrate are washed using deionized water. USE - Method for transferring graphene into a flexible substrate. ADVANTAGE - The method enables ensuring simple operation and wide application range, avoiding damage of graphene material, realizing high efficiency and reducing processing cost. DESCRIPTION OF DRAWING(S) - The drawing shows a sectional view of a flexible substrate.