• 专利标题:   Titanium-based polymer alloy copolymer used for preparing titanium-based polymer alloy heat exchanger coating comprises soluble imide resin, hydroxyl organic titanium polymer, N-methylpyrrolidone and dimethylacetamide.
  • 专利号:   CN112390958-A
  • 发明人:   YI J, PENG X, ZHANG C, ZHOU J, TANG S, KUANG Z, ZHONG H, YE Y, LUO H, ZHANG S
  • 专利权人:   ZEYI FOSHAN IND TECHNOLOGY CO LTD
  • 国际专利分类:   C08G079/00, C08G081/00, C09D187/00, C09D005/08, C09D005/10
  • 专利详细信息:   CN112390958-A 23 Feb 2021 C08G-081/00 202128 Pages: 18 Chinese
  • 申请详细信息:   CN112390958-A CN10069966 19 Jan 2021
  • 优先权号:   CN10069966

▎ 摘  要

NOVELTY - A titanium-based polymer alloy copolymer comprises 400-500 pts. wt. soluble imide resin, 100-300 pts. wt. hydroxyl organic titanium polymer, 50-200 pts. wt. N-methylpyrrolidone and 100-300 pts. wt. dimethylacetamide. The soluble imide resin is polyimide resin, polyamide-imide resin, and/or bismaleimide resin. USE - The titanium-based polymer alloy copolymer is used for preparing titanium-based polymer alloy heat exchanger coating (claimed). DETAILED DESCRIPTION - A titanium-based polymer alloy copolymer comprises 400-500 pts. wt. soluble imide resin, 100-300 pts. wt. hydroxyl organic titanium polymer, 50-200 pts. wt. N-methylpyrrolidone and 100-300 pts. wt. dimethylacetamide. The soluble imide resin is polyimide resin, polyamide-imide resin, and/or bismaleimide resin. The hydroxyl organic titanium polymer is of formula (I). INDEPENDENT CLAIMS are included for: (1) preparation of the alloy copolymer comprising taking imide resin, N-methyl pyrrolidone, and dimethyl acetamide, mixing, stirring, heating until the imide resin is completely dissolved, adding hydroxyl organic titanium polymer, raising temperature to 100-140 degrees C, and reacting for 2-4 hours at constant temperature; (2) titanium-based polymer alloy heat exchanger aqueous coating comprising 10-15 pts. wt. titanium-based polymer alloy copolymer, 5-10 pts. wt. aqueous phenyl silicone resin, 5-10 pts. wt. water-soluble phenolic resin, 10-15 pts. wt. aqueous epoxy emulsion, 2-5 pts. wt. tetrahydrofuran, 5-10 pts. wt. aqueous graphene dispersion slurry with solid content of 5-10%, 20-25 pts. wt. antirust pigment, 10-20 pts. wt. co-curing agent, and 2.5-5 pts. wt. coating auxiliary agent; and (3) titanium-based polymer alloy heat exchanger oil coating comprising 15-20 pts. wt. titanium-based polymer alloy copolymer, 5-10 pts. wt. epoxy resin, 5-8 wt.% to 8 parts of phenoxy resin, 3-5 pts. wt. elastomer polyester resin, 5-8 pts. wt. liquid fluorine-silicone rubber, 10-20 pts. wt. co-curing agent, 5-10 pts. wt. oily graphene dispersion slurry with solid content of 5-10%, 2-5 pts. wt. propylene glycol methyl ether acetate, 2-5 pts. wt. diacetone alcohol, 2-5 pts. wt. methyl isobutyl ketone, 20-25 pts. wt. antirust pigment, 5-15 pts. wt. pigment filler, and 2-5 pts. wt. coating auxiliary agent.