▎ 摘 要
NOVELTY - A corrosion-resistant solar energy-absorbing coating comprises 10-20 mass parts PTFE emulsion, 5-12 mass parts alkyd resin, 8-14 mass parts acetyl tributyl citrate, 10-20 mass parts nano-silicon micropowder, 5-14 mass parts graphene, 5-10 mass parts N-ethylcarbazole, 6-12 mass parts ethyl acetate, 10-24 mass parts ethanol, and 20-28 mass parts water. USE - A corrosion-resistant solar energy-absorbing coating (claimed). ADVANTAGE - Corrosion-resistant solar energy-absorbing coating has good solar energy absorptivity and good water resistance. Production process is simple and easy. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for production of corrosion-resistant solar energy-absorbing coating which involves adding PTFE emulsion, alkyd resin, and N-ethylcarbazole, warming at 100-110 degrees C, stirring for 1-3 hours, adding nano-silicon micropowder and mass parts graphene, stirring for 20-30 minutes to obtain mixture A, mixing ethanol and water, dropping mixture A, stirring, adding acetyl tributyl citrate, stirring, and naturally cooling.