▎ 摘 要
NOVELTY - Degradable butyronitrile latex comprises 400-600 pts. wt. butyronitrile latex, 4-12 pts. wt. modified graphene oxide, 24-36 pts. wt. modified talcum powder, 12-26 pts. wt. micro-material, 8-16 pts. wt. vulcanizing agent, 7-14 pts. wt. zinc oxide, 2-6 pts. wt. cross-linking agent, 3-6 pts. wt. stabilizing agent, 1-4 pts. wt. dispersant. USE - Degradable butyronitrile latex used for glove. ADVANTAGE - The degradable butyronitrile latex has better tensile strength, wear resistance, cutting resistance, acid and alkali resistance, and easy degradation. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is inluded for a method for preparing degradable butyronitrile latex, which involves: (A) weighing each raw material; (B) mixing the modified graphene oxide, modified talcum powder and micro-material, putting into ball mill to grind to obtain mixed powder; and (C) mixing the mixed powder, butyronitrile latex, vulcanizing agent, zinc oxide, cross linking agent, stabilizing agent and dispersing agent to obtain the product.