▎ 摘 要
NOVELTY - Improved artificial stone comprises 50-60 wt.% silica, 25-35 wt.% aluminum oxide, 6-10 wt.% potassium oxide, 0.2-0.4 wt.% calcium oxide, 0-0.5 wt.% iron oxide, 0.03-0.05 wt.% magnesium oxide, and 2-5 wt.% graphene. USE - Improved artificial stone. ADVANTAGE - The material is slightly translucent, and has high strength and improved wear resistance. The preparation method is easy and has low production costs. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for the preparation of improved artificial stone comprising mixing raw materials at 800-1000 revolutions/minute for 10-25 minutes, pressing, forming, sintering, and cooling.