• 专利标题:   Preparing waffle shape adsorbent composite material comprises selecting ionic liquid with carboxylate, adding the ionic liquid into N,N-dimethylmethanamide aqueous solution, adding the graphene oxide solution, dissolving trimesic acid in DMF solution, condensing and refluxing.
  • 专利号:   CN115025761-A
  • 发明人:   LU C, WANG L, LI A, LI L, WU G, ZHANG F, HE C, KONG F, BIAN Z
  • 专利权人:   XIAN THERMAL POWER RES INST CO LTD, SUZHOU XIRE ENERGY CONSERVATION ENVIRO
  • 国际专利分类:   B01D053/02, B01D053/86, B01J020/22, B01J020/28, B01J020/30, B01J031/22
  • 专利详细信息:   CN115025761-A 09 Sep 2022 B01J-020/22 202297 Chinese
  • 申请详细信息:   CN115025761-A CN10542692 18 May 2022
  • 优先权号:   CN10542692

▎ 摘  要

NOVELTY - Preparing waffle shape adsorbent composite material comprises (1) using graphite, sodium nitrate, concentrated sulfuric acid, potassium permanganate and hydrogen peroxide to prepare graphene oxide solution, (2) selecting ionic liquid with carboxylate, adding the ionic liquid into N,N-dimethylmethanamide aqueous solution, stirring for a period of time, adding the graphene oxide solution obtained in step (1), the volume ratio of the graphene oxide solution and the ionic liquid is 1: 1-10, ultrasonically dispersing to obtain GO-IL solution, (3) dissolving the trimesic acid (H3BTC) in DMF solution, obtaining the first precursor solution, dissolving cupric nitrate Cu (NO3) 2 in the deionized water to obtain the second precursor solution, mixing first and second precursor solution with the GO-IL solution, condensing and refluxing for a period of time in the oil bath to obtain the mixture, filtering the mixture, washing and drying. USE - The method is useful for preparing waffle shape adsorbent composite material. DETAILED DESCRIPTION - Preparing waffle shape adsorbent composite material comprises (1) using graphite, sodium nitrate, concentrated sulfuric acid, potassium permanganate and hydrogen peroxide to prepare graphene oxide solution, (2) selecting ionic liquid with carboxylate, adding the ionic liquid into N,N-dimethylmethanamide aqueous solution, the volume ratio of ionic liquid and DMF aqueous solution is 1: 40-200, stirring for a period of time, adding the graphene oxide solution obtained in step (1), the volume ratio of the graphene oxide solution and the ionic liquid is 1: 1-10, ultrasonically dispersing to obtain GO-IL solution, (3) dissolving the trimesic acid (H3BTC) in DMF solution, obtaining the first precursor solution, dissolving cupric nitrate Cu (NO3) 2 in the deionized water to obtain the second precursor solution, mixing first and second precursor solution with the GO-IL solution obtained in step (2) according to the volume ratio of 20-80: 10-50: 10-50, condensing and refluxing for a period of time in the oil bath to obtain the mixture, filtering the mixture, washing, drying to obtain the final product GO-IL/MOF.