▎ 摘 要
NOVELTY - Loading visible light in response to titanium dioxide by graphene comprises disposing the acid-water mixed solution, adding the graphene oxide nano-powder, ultrasonically dispersing for 5-60 minutes to obtain a uniform graphene oxide dispersion, adding titanium alkoxide, where the adding amount of the titanium dioxide is 1-50 wt.% of the amount of the acid-water mixed solution, stirring, heating to 50-95 degrees C for 1-5 hours, cooling to room temperature for 10-20 hours to obtain a graphene-supported visible light response titanium dioxide. USE - The method is useful for loading visible light in response to titanium dioxide by graphene. ADVANTAGE - The method is simple.