▎ 摘 要
NOVELTY - A nitro-containing organic explosive is mixed with component containing carbon and nitrogen in mass ratio of 1 to 5:1, obtained mixture is provided into sealed stainless steel reactor with packing density of 0.06-0.25 g/ml, heated at 220-420 degrees C, cooled and gases are discharged, to obtain nitrogen-doped graphene. USE - Method for preparing nitrogen-doped graphene. ADVANTAGE - The method economically provides nitrogen-doped graphene in high yield, using simple process.