▎ 摘 要
NOVELTY - High-temperature-resistant graphite alkenyl mono-component epoxy anti-corrosive coating comprises 100 pts. wt. epoxy resin, 10-20 pts. wt. amino-polysiloxane, 10-30 pts. wt. toughening agent, 0.1-3 pts. wt. graphene, 20-50 pts. wt. reactive diluent, 0.1-0.3 pt. wt. silane coupling agent, 0.1-2 pts. wt. dispersant, 0-2 pts. wt. pigment, 12-18 pts. wt. boron trifluoride-amine complex and 5-12 pts. wt. dicyandiamide. USE - High-temperature-resistant graphite alkenyl mono-component epoxy anti-corrosive coating used for high temperature pipeline (claimed). ADVANTAGE - The coating has high toughness and wear resistance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the high-temperature-resistant graphite alkenyl mono-component epoxy anti-corrosive coating comprising mixing epoxy resin, amino-polysiloxane, toughening agent, graphene, reactive diluent, silane coupling agent, dispersant, pigment, boron trifluoride-amine complex and dicyandiamide.