▎ 摘 要
NOVELTY - Semi-aromatic polyamide resin comprises 5000-10000 pts. wt. semi-aromatic polyamide salt solution, 50-500 pts. wt. graphene oxide water solution, and 7-15 pts. wt. auxiliary agent. USE - Semi-aromatic polyamide resin. ADVANTAGE - The semi-aromatic polyamide resin has m.pt. of 270-310 degrees C, glass transition temperature of 90-110 degrees C, relative viscosity of 2-2.8, improved mechanical property, electrical property, and thermal conductivity. The method is cost-effective and has a yield of 98.4%. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of resin comprising reacting raw materials at high temperature and high pressure to obtain prepolymer, carrying out high temperature vacuum prepolymer reaction; extruding and granulating.