▎ 摘 要
NOVELTY - Graphene oxide antibacterial shampoo comprises 10-50 wt.% surfactant, 0.5-12 wt.% graphene oxide, 0.5-10 wt.% thickener, 0.05-0.3 wt.% citric acid, 0.02-0.6 wt.% yeast/rice fermentation product filtrate, 0.04-1 wt.% golden chamomile extract, 0.02-0.8 wt.% lauryl dimethyl ammonium hydroxypropyl hydrolyzed collagen, 0.04-2 wt.% flavor panthenol, and 0.01-0.3 wt.% deionized water. USE - Graphene oxide antibacterial shampoo. ADVANTAGE - The graphene oxide antibacterial shampoo effectively inhibit the reproduction of Malassezia, achieve physical antibacterial and antibacterial properties, has anti-dandruff and antipruritic effect is obvious. The shampoo is mild, green and safe, can effectively inhibit bacteria and has no side effects on the human body, the preparation process is simple, convenient to operate, environmentally friendly, suitable for large-scale industrial promotion, and the produced graphene shampoo can effectively inhibit bacteria, and overcome the problem of anti-dandruff and anti-itch. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing graphene oxide antibacterial and antibacterial shampoo, which comprises (A) weighing the components according to the formula, preparing graphene oxide into graphite oxide, adding graphene oxide dispersion and surfactant to deionized water in sequence, and stirring, putting the well-stirred mixture into a homogeneous dispersing emulsifier, and heating up to 40-80 degrees C at 800-1500 rpm, and stirring at constant speed for 20-30min, adding thickener, cooling to 60-40 degrees C, setting the stirring speed to 800-1500rpm for 10-30min, making the mixture fully dissolved under the action of strong shearing force, and reaching emulsification and homogeneity; (B) adding flavor, stirring at 500-1000rpm for 10-20min, and cooling to room temperature; and (C) adding citric acid, yeast/rice fermentation product filtrate, golden chamomile extract, lauryl dimethyl ammonium hydroxypropyl hydrolyzed collagen, panthenol, adjusting the pH to 6.5-7.2, and stirring to obtain graphene oxide antibacterial and antibacterial shampoo.