• 专利标题:   Skin-friendly antibacterial towel is woven by yarns of polymerized and optimized graphene polyamide fiber, polytrimethylene terephthalate fiber, coffee carbon fiber, modal fiber, bamboo pulp fiber, viscose fiber and water-soluble vinylon.
  • 专利号:   CN108060500-A
  • 发明人:   ZHANG W, HUANG X
  • 专利权人:   JIANGSU ENG TECHNOLOGY COLLEGE
  • 国际专利分类:   D03D013/00, D03D015/00, D03D015/06, D03D027/08, D06M101/06, D06M101/24, D06M101/32, D06M101/34, D06M011/38, D06M011/76, D06M013/207, D06M015/643
  • 专利详细信息:   CN108060500-A 22 May 2018 D03D-027/08 201842 Pages: 7 Chinese
  • 申请详细信息:   CN108060500-A CN11340828 14 Dec 2017
  • 优先权号:   CN11340828

▎ 摘  要

NOVELTY - Skin-friendly antibacterial towel is woven by yarns of a polymerized and optimized graphene polyamide fiber, a polytrimethylene terephthalate (PTT) fiber, a coffee carbon fiber, a modal fiber, a bamboo pulp fiber, a viscose fiber, a water-soluble vinylon, hair warp yarn 10-21S, ground warp yarn 21S-32S double strand, and weft yarn 14S-21S. The density is 300-400 pieces per 10cm, and weft density is 150-200 pieces/10cm. The weight of fabric is 75g-95g/bar, and the towel is subjected to extraction, dyeing and drying process. The finished product has a specification of 32-35cmx 68-75cm. USE - Skin-friendly antibacterial towel. ADVANTAGE - The skin-friendly antibacterial towel has simple preparation process, elasticity, flexibility, anti-bacterial effect, good application prospect, and is suitable for mass production. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a skin-friendly antibacterial towel, which involves: (A) carding, combing, drawing and carrying out rough spinning of warp yarn and weft yarn according to spinning process to obtain the mixed yarn; (B) twisting mixed yarn at a rate of 45-60 twist/10cm, using high-speed flat-press batch warping machine to warp the warp and grounded warp yarns respectively to make hair warp beam and ground warp beam; and (C) carrying out sizing process by using slurry which is a modified starch slurry at a sizing rate of 2-6%, obtaining raw yarn by using a weaving towel having height of 4.8-5.1mm, hair ratio is 4-7 times and loom speed of 320-520 revolutions per minute to obtain 75g-95g/bar towel semi-finished products.