▎ 摘 要
NOVELTY - Graphene paint comprises 30-70 wt.% prepolymer, 25-60 wt.% monomer, 1-10 wt.% photoinitiator, 0-10 wt.% additive and graphene, where the addition amount of graphene is 10-10000 parts per million. USE - The graphene paint is useful for surface treatment of optical film in display (claimed). ADVANTAGE - The graphene paint: maintains the properties of the resin itself; reduces the water vapor transmission rate after the coating is cured; has light transmittance in the range of 400-450 nm and antistatic effect, transmittance of the coating formed by the graphene paint of 400-450 nm, and transmittance of 1-70%; water vapor transmission rate of 10-300 g/m for 2.24 hours, and surface resistance of 105-1012 Omega . DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for use of graphene paint comprising mixing prepolymer, monomer, photoinitiator and additive, stirring at room temperature, adding graphene having a diameter of 5-50 mu m, ball milling for 5-7 hours, coating the ball-milled graphene paint on the surface of the TAC film, coating thickness 7 plus minus 2 mu m, allowing to stand at room temperature for 2-4 minutes, and curing the graphene paint using high pressure mercury lamp.