• 专利标题:   Preparing graphene nanofiltration membrane, by adding prepared graphene dispersion to solvent, adding layer spacing regulator, reacting, adding homemade graphene, forming nanofiltration membrane and drying membrane.
  • 专利号:   CN106964263-A
  • 发明人:   HU K, LI X, QU L, SONG Y, YU W, ZHANG M, ZHANG Z, ZHENG G
  • 专利权人:   SHANDONG JINCHENG GRAPHENE TECHNOLOGY CO
  • 国际专利分类:   B01D061/00, B01D067/00, B01D069/02, B01D069/10, B01D071/02, C02F001/44
  • 专利详细信息:   CN106964263-A 21 Jul 2017 B01D-071/02 201761 Pages: 9 Chinese
  • 申请详细信息:   CN106964263-A CN10286161 27 Apr 2017
  • 优先权号:   CN10286161

▎ 摘  要

NOVELTY - Method for preparing solvent resistant, stain resistant, graphene nanofiltration membrane, involves adding 0.2-0.4 ml prepared graphene dispersion to 30 ml solvent, adding layer spacing regulator to the mixture, reacting the mixture at 40-60 degrees C for 2-4 hours, cooling the mixture to room temperature, adding 0.07-0.12 mg/ml homemade graphene to the mixture, forming nanofiltration membrane having a graphene separation layer on the surface of the polymer membrane by filtration, spin coating, spraying or brushing process, and drying the membrane. USE - The method is useful for preparing solvent resistant, stain resistant, graphene nanofiltration membrane which is used in treatment and desalination of sewage (all claimed). ADVANTAGE - The method prolongs service life. DETAILED DESCRIPTION - Method for preparing solvent resistant, stain resistant, graphene nanofiltration membrane, involves adding 0.2-0.4 ml prepared graphene dispersion to 30 ml solvent, adding layer spacing regulator to the mixture, reacting the mixture at 40-60 degrees C for 2-4 hours, cooling the mixture to room temperature, adding 0.07-0.12 mg/ml homemade graphene to the mixture, forming nanofiltration membrane having a graphene separation layer on the surface of the polymer membrane by filtration, spin coating, spraying or brushing process, and drying the membrane at room temperature or in storage solvent, where the amount of graphene loaded in the nanofiltration membrane is 20-68 mg/m2.