▎ 摘 要
NOVELTY - Insect repellent aqueous paint composite material comprises 40-50 pts. wt. aqueous acrylic resin emulsion, 4-5 pts. wt. cellulose acetate, 0.1-0.2 pts. wt. polyoxyethylene alkyl ether, 0.1-0.2 pt. wt. borneol, 0.8-1 pt. wt. expanded graphite powder, 0.01-0.02 pt. wt. graphene oxide, 0.1-0.2 pt. wt. silane coupling agent, 0.1-0.2 pt. wt. silicon antifoaming agent, 15-20 pts. wt. N,N-dimethylformamide, 30-40 pts. wt. acetone, 10-12 pts. wt. anhydrous ethanol and deionized water. USE - Insect repellent aqueous paint. ADVANTAGE - The insect repellent aqueous paint has good aroma, good absorbability, good dispersibility and excellent performance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of insect repellent aqueous composite material comprising mixing expanded graphite powder, graphene oxide and silane coupling agent in absolute ethanol and deionized water, stirring, heating at 60-65 degrees C, reacting for 4-6 hours , drying at 250-300 degrees C for 1.5-2 hours under nitrogen gas, adding cellulose acetate and borneol, subjecting to ultrasonic vibration for 6-8 hours, electrospinning at 400-500 revolutions/minute, centrifuging, drying to obtain composite cellulose nanofiber, adding aqueous acrylic emulsion and balance raw materials, adjusting viscosity and screening.