▎ 摘 要
NOVELTY - An active porous graphene is prepared by taking graphene oxide, adding mixed solution, adjusting pH value to 9-10, stirring for 1-10 hours, ultrasonically dispersing for 0.5-2 hours to obtain colloidal graphene oxide dispersion, adding solid chemical foaming agent, stirring for 2-12 hours, filtering to remove excess solid chemical foaming agent, and drying. USE - Method for preparing active porous graphene (claimed).