▎ 摘 要
NOVELTY - Graphite heat insulation lightweight paint comprises 7-10 pts. wt. calcium carbonate, 3-5 pts. wt. talcum powder, 3-5 pts. wt. gypsum powder, 15-25 pts. wt. titanium dioxide, 0.5-2 pts. wt. fumed silica, 2-4 pts. wt. graphene powder, 0.1-1 pts. wt. surface active agent, 0.01-0.1 pts. wt. antifoaming agent, 3-8 pts. wt. film forming agent, 0.02-0.1 pts. wt. sterilization fungicide and 30-90 pts. wt. water. USE - Graphite heat insulation lightweight paint is used for wall paint or heat-resistant wall paint (claimed). ADVANTAGE - The graphite heat insulation lightweight paint has good adhesion property,firm and firm frame, super-durability, good heat insulation performance, and convenient transportation and coating. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing a graphene heat insulation lightweight paint, which involves: (A) selecting particle size of calcium carbonate, talcum powder, gypsum powder, titanium dioxide and fumed silica are mixing and stirring uniformly at suitable conditions to obtain mixture; (B) dissolving the obtained mixture into surfactant, film forming agent, sterilization fungicide and deionized water and stirring uniformly at suitable conditions to obtain composite; and (C) dissolving the obtained composite into graphene powder and the antifoaming agent, and stirring for 10-30 minutes to obtain the desired product.