NOVELTY - A decorative item of still life is decorated by covering an element of nature, applying electrically conductive layer, applying gold layer, applying initial stiffening layer in the form of paint with metallic particles to the still life element, drying, applying second proper stiffening layer of epoxy resin with a hardener at a concentration of 10:1 components with the addition of graphene nanoparticles (reduced graphene oxide) or carbon nanotubes, leaving to dry for 24 hours, covering with electroconductive paint with nanosilver particles, leaving for about 30 minutes until fully dry, carrying out galvanic gold plating at 45-50 degrees C, voltage of 15-17 V, and current intensity of 0.05 A for 15-30 minutes, drying, polishing with swabs soaked in a gilding bath at 45-50 degrees C, and coating a protective layer. The composition of the proper stiffening layer contains 100 ml epoxy resin (Epidian 5), 10 ml hardener, and 0.05 g reduced graphene oxide or carbon nanotubes. USE - The method is useful for decorating a decorative item of still life. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for backing layer stiffening composition for use in the method for decorating a decorative item of still life.