▎ 摘 要
NOVELTY - The graphene composite rubber-asphalt mixture comprises 80-100 parts petroleum asphalt, 5-8 parts rubber powder, 80-100 parts aggregate, 1-5 parts graphene composite material, 0.1-0.2 part polyethylene wax, 0.35-1 part triethyloleate, and 0.3-1.5 parts aromatic oil. USE - Graphene composite rubber-asphalt mixture is used in high-grade highways. ADVANTAGE - The graphene composite material rubber asphalt mixed material has high dynamic stability and marshal strength and has obvious anti-rutting performance and anti-shearing performance. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for the preparation of the graphene composite rubber-asphalt mixture.