▎ 摘 要
NOVELTY - Outdoor textile coating glue comprises 50-80 pts. wt. of polyrotaxanes, 10-12 pts. wt. of polysaccharides, 20-30 pts. wt. of polymer compounds, 5-8 pts. wt. of phenols, and 0.02-5 pts. wt. of catalysts, 1-10 pts. wt. of auxiliary, 8-10 pts. wt. of carbon material, 150-200 pts of dimethyl sulfoxide, 200-400 pts. wt. of deionized water. USE - Outdoor textile coating glue. ADVANTAGE - The outdoor textile coating glue has excellent UV light absorption and utilization, is capable of responding to some long-time outdoor strong sunlight irradiation condition, and has excellent outdoor service life, and good production and use prospect. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for the method for preparing textile coating glue, which involves: 1. dissolving polyrotaxane macromolecule compound polysaccharide in dimethyl sulfoxide adding catalyst stirring and reacting for 5-6 hours at 85℃; 2. washing and filtering after finishing reaction removing solvent and impurity; 3. adding proper amount of auxiliary agent carbon material deionized water and phenols stirring for 1-2 hours to obtain the outdoor textile coating glue.