▎ 摘 要
NOVELTY - A porous modified graphene oxide film is prepared by using 35-50 pts. wt. porous modified graphene oxide, 25-35 pts. wt. porous ceramics, 50-70 pts. wt. solvent (A), and 55-75 pts. wt. solvent (B), dispersing the porous modified graphene oxide in the solvent (A) to obtain a dispersion liquid, and scraping a film to obtain a porous modified graphene oxide liquid membrane, adding the prepared porous modified graphene oxide liquid membrane and porous ceramics to the solvent (B) and soaking for 20 hours to prepare a porous modified graphene oxide gel membrane, and drying the prepared film. USE - Porous modified graphene oxide film. ADVANTAGE - The porous modified graphene oxide film has increased pore size.