▎ 摘 要
NOVELTY - Anti-radiation paint comprises 2-4 wt.% molybdenum disulfide, 6-10 wt.% graphene oxide, 7-25 wt.% silicone resin, 10-15 wt.% butyl acetate, 3-5 wt.% nano boron nitride, 4-19 wt.% nano alumina, 4-6 wt.% titanium dioxide, 3-5 wt.% antifoaming agent, 4-8 wt.% antibacterial agent and 20-40 wt.% de-ionized water. USE - Anti-radiation paint for computer. ADVANTAGE - The anti-radiation paint has better anti-radiation effect and heat resistance property. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing anti-radiation paint, which involves: (A) mixing graphene oxide, silicone resin, butyl acetate, nano Boron nitride, nano-alumina, and molybdenum disulfide; (B) adding deionized water gradually; (C) pouring into a sand mill to grind and stir, until the solution particle size is 10-30 microns; (D) adding titanium oxide, antifoaming agent and bacteriostatic agent to the mixture; (E) stirring at 60-80 degrees C for 20-50 minutes; and (F) cooling the obtained mixture.