▎ 摘 要
NOVELTY - High building composite material comprises 22-46 pts. wt. modified graphene oxide, 18-35 pts. wt. silica powder, 5-15 pts. wt. inorganic fiber, 3-8 pts. wt. chromium oxide green, 6-12 pts. wt. anhydrous active limestone, 4-10 pts. wt. vanadium diboride, 3-5 pts. wt. active magnesium oxide, 3-9 pts. wt. crystalline flake graphite, and 0.1-4 pts. wt. adhesive. USE - High building composite material. ADVANTAGE - The material can resist heat at up to 1600 degrees C. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the high building composite material comprising mixing raw materials, ball milling, and hot pressing.