▎ 摘 要
NOVELTY - Paint comprises 1-20 pts. wt. graphene-based nanoscale zero valent iron, 1-15 pts. wt. nano titanium dioxide, 1-15 pts. wt. nano graphene oxide, 1-15 pts. wt. graphene nano silica, 1-15 pts. wt. nano calcium carbonate, 5-60 pts. wt. epoxy resin, 3-30 pts. wt. polyphenylene sulfide resin, 1-15 pts. wt. amino resin crosslinking agent, 3-50 pts. wt. solvent, 0.5-1.9 pts. wt. nonionic surfactants, 0.8-1.6 pts. wt. dispersant, 0.5-1.5 pts. wt. thickener, 0.1-0.3 pts. wt. defoamers, 0.1-5 pts. wt. plasticizer, 0.2-0.5 pts. wt. leveling agent, 1-10 pts. wt. pigment and 0.5-1.0 pts. wt. filler. USE - Paint. ADVANTAGE - The paint has heat, corrosion, weather, adhesion and chemical resistance properties. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing paint, which involves: (A) mixing graphene-based nanoscale zero valent iron, silicon dioxide, graphene nano calcium carbonate, epoxy resin and polyphenylene sulfide resin; (B) stirring the mixture for 35-280 minutes; (C) adding filler and pigment in the stirred mixture; (D) stirring the mixture for 10-150 minutes; (E) adding active agent, dispersing agent, thickening agent, defoaming agent, plasticizer and flatting agent in the mixture; (F) stirring the mixture for 35-200 minutes; (G) adding amino resin crosslinking agent in the mixture; (H) stirring the mixture for 15-200 minutes; and (I) filtering the mixture.