▎ 摘 要
NOVELTY - An activated graphene for super capacitor is prepared by microwave heating graphite powder at 1-50 MPa and 600-2000 W for 10-600 seconds, pore-forming on graphene surface, adding gas or liquid in reaction kettle, entering into supercritical fluid state, and optimizing physical chemical parameter. USE - Method for preparing activated graphene for super capacitor (claimed).