▎ 摘 要
NOVELTY - Styrene-butadiene-styrene elastomer modified asphalt waterproof coiled material comprises waterproof coiled material base layer, modified asphalt layer and isolation layer. The modified asphalt layer comprises 50 pts. wt. No. 130 asphalt, 40 pts. wt. No. 90 asphalt, 7 pts. wt. sodium hexametaphosphate, 10 pts. wt. styrene-butadiene-styrene, 5 pts. wt. paraffin oil, 2 pts. wt. antioxidant, 6 pts. wt. graphene, 7 pts. wt. petroleum resin, 5 pts. wt. coumarone resin, 2 pts. wt. glycerin monostearate, 4 pts. wt. oleic acid amide, 0.3 pts. wt. anti-aging agent and 15 pts. wt. filler. The filler is calcium carbonate and/or calcium silicate. USE - Used as styrene-butadiene-styrene elastomer modified asphalt waterproof coiled material. ADVANTAGE - The styrene-butadiene-styrene elastomer-modified asphalt waterproof coiled material has excellent heat preservation property, heat insulation property, water resistance, weather resistance, aging resistance and corrosion resistance.