▎ 摘 要
NOVELTY - Processing blended wool graphene material, comprises e.g. (a) equipping with treatment box with a concentration of 2-3% chlorinated liquid in the treatment box, dipping the wool into processing box, (b) adding 2-7 wt.% wool wt. sodium sulfite in the treatment box, (c) adding 1-2 wt.% wool wt. protease in the treatment box, (d) washing using clean water to remove the dirt attached to the surface of wool, (i) equipping with bath box, there is water-soluble graphene soaking solution with a concentration of 0.2-1% in the soaking bath, (ii) soaking wool cleaned in step (iv) into soaking liquid, soaking, (iii) dehydrating wool and drying, and carrying out second bath (iv) there is generator cabinet with a water-soluble graphene generator with a concentration of 0.8-1.5%, (v) dipping the dried grey cloth into generating liquid, soaking, using ultrasound to apply vibration, and (vi) drying the grey cloth in the cabinet after dehydration. USE - The method is useful for processing blended wool graphene woolen material. ADVANTAGE - The material: has excellent antistatic function, excellent antibacterial and antibacterial effect and excellent air permeability. DETAILED DESCRIPTION - Processing blended wool graphene material, comprises (a) equipping with treatment box with a concentration of 2-3% chlorinated liquid in the treatment box, dipping the wool into processing box, the mass of chlorinated solution is 0.5-1.5 wt.% of wool wt. the processing temperature is 21-25 degrees C, soaking for 45-75 minutes, (b) adding 2-7 wt.% wool wt. sodium sulfite in the treatment box, the processing temperature is 20-30 degrees C, processing time is 45-60 minutes, (c) adding 1-2 wt.% wool wt. protease in the treatment box, the processing temperature is 40-60 degrees C, processing time is 1.5-3 hours, (d) washing using clean water to remove the dirt attached to the surface of wool, (i) equipping with bath box, there is water-soluble graphene soaking solution with a concentration of 0.2-1% in the soaking bath, (ii) soaking the wool cleaned in step (iv) into soaking liquid, soaking for 1.5-2.5 hours, the soaking temperature is 35-55 degrees C, (iii) dehydrating wool and drying, and carrying out second bath (iv) there is generator cabinet with a water-soluble graphene generator with a concentration of 0.8-1.5%, (v) dipping the dried grey cloth into generating liquid, soaking for 50-70 minutes, the soaking temperature is 35-45 degrees C, using ultrasound to apply vibration, and (vi) drying the grey cloth in the cabinet after dehydration.