▎ 摘 要
NOVELTY - Preparation of paint involves drying 40-60 pts. wt. tungsten-cobalt carbide powder, drying, obtaining dried tungsten-cobalt carbide powder, adding 20-30 pts. wt. epoxy resin, 1 pt. wt. silane coupling agent, 20-30 pts. wt. ethanol and 3-7 pts. wt. benzyl alcohol, mixing, obtaining epoxy resin mixture, adding mixture comprising 20-30 pts. wt. polyamide, 7-13 pts. wt. benzyl alcohol and 0.7-1.3 pts. wt. graphene and mixing uniformly. USE - Preparation of paint (claimed). ADVANTAGE - The method provides paint by economical process. The film obtained using the paint has excellent wear resistance.