▎ 摘 要
NOVELTY - Acceleration of II-I crystal form transformation of isotactic polybutylene-1 involves adding 0.01-0.09 %mass graphene to isotactic polybutylene-1 in fusion state, and melt-blending at 150-180 degrees C. USE - Acceleration of II-I crystal form transformation of isotactic polybutylene-1 used for improving mechanical properties (claimed). ADVANTAGE - The method provides II-I crystal form-transformed isotactic polybutylene-1 having excellent tensile strength and impact performance.