• 专利标题:   Solid rubber tire comprises natural rubber, nitrile rubber, polybutadiene, hydroxyethyl acrylate, graphene, nano-titanium dioxide, stearic acid, antioxidant, vulcanizing agent, coupling agent, and filler, which has good forming effect.
  • 专利号:   CN107099064-A
  • 发明人:   BIAN Z
  • 专利权人:   MINGGUANG SUNAIDE SOLID TYRE CO LTD
  • 国际专利分类:   B60C001/00, C08K013/02, C08K003/04, C08K003/22, C08K003/34, C08K005/09, C08K005/101, C08K005/54, C08L047/00, C08L007/00, C08L009/02
  • 专利详细信息:   CN107099064-A 29 Aug 2017 C08L-007/00 201776 Pages: 6 Chinese
  • 申请详细信息:   CN107099064-A CN10410068 03 Jun 2017
  • 优先权号:   CN10410068

▎ 摘  要

NOVELTY - Solid rubber tire comprises 35-50 pts. wt. natural rubber, 5-12 pts. wt. nitrile rubber, 10-20 pts. wt. polybutadiene, 9-18 pts. wt. hydroxyethyl acrylate, 2-7 pts. wt. graphene, 5-8 pts. wt. nano-titanium dioxide, 6-13 pts. wt. stearic acid, 3-9 pts. wt. antioxidant, 5-10 pts. wt. vulcanizing agent, 6-10 pts. wt. coupling agent, and 15-23 pts. wt. filler. USE - Solid rubber tire. ADVANTAGE - The solid rubber tire has good forming effect, good wear resistance, corrosion resistance, and weather resistance, which ensures safety of the vehicle. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for a method for preparing solid rubber tire, which involves: (A) mixing natural rubber, nitrile rubber, and polybutadiene at rate of 70-85 revolutions/minute; (B) plasticating at 58-63 degrees C for 80-100 seconds to obtain mixture a1; (C) adding graphene, hydroxyethyl acrylate, and silane coupling agent into mixture a1 and mixing for 80-90 seconds, adding nano-titanium dioxide, antioxidant, and filler ; (D) mixing for 80-90 seconds at room temperature; (E) mixing with vulcanizing agent and stearic acid, mixing for 50-55 seconds; (F) mixing for 5-10 seconds; and (G) kneading mixture to obtain solid rubber.