• 专利标题:   Putty powder comprises e.g. stone powder, cement, active diluting agent, emulsifier, epoxy resin, rosin saponified material, palm oil, carboxymethyl cellulose, copper fiber powder, graphene composite material, and anti-freezing agent.
  • 专利号:   CN107603323-A
  • 发明人:   CHEN W
  • 专利权人:   CHEN W
  • 国际专利分类:   C09D005/34
  • 专利详细信息:   CN107603323-A 19 Jan 2018 C09D-005/34 201817 Pages: 11 Chinese
  • 申请详细信息:   CN107603323-A CN11065554 02 Nov 2017
  • 优先权号:   CN11065554

▎ 摘  要

NOVELTY - Putty powder comprises 30-50 pts. wt. stone powder, 12-20 pts. wt. cement, 5-20 pts. wt. active diluting agent, 4-20 pts. wt. emulsifier, 3-16 pts. wt. epoxy resin, 2-10 pts. wt. rosin saponified material, 0.5-5 pts. wt. palm oil, 1-10 pts. wt. carboxymethyl cellulose, 0.2-3 pts. wt. copper fiber powder, 0.05-1 pts. wt. graphene composite material, 0.1-1 pts. wt. polyvinyl alcohol powder, and 1-5 pts. wt. anti-freezing agent. USE - Used as putty powder. ADVANTAGE - The putty powder: has good fluidity, water retention frost resistance, and strong adhesive force; and avoids phenomena of water spots, white spots, and rust spots. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the putty powder comprising (i) taking abandoned stone powder, adding into the feeder, crushing, adding into drier, drying passing through 200-300 mesh sieves to obtain powder material; (ii) adding rosin, sodium hydroxide and water into the reaction kettle, heating at 160-190 degrees C for 20-40 minutes to obtain brown transparent paste, placing the paste in vacuum dryer, drying at 60-80 degrees C under pressure 93.3-98.6 KPa for 5-7 hours, and grinding to obtain rosin saponified material; (iii) adding the cement and powder material obtained in step (i) into putty powder mixer, stirring for 1-2 minutes under dry state, adding active diluting agent, epoxy resin, emulsifier, carboxymethyl cellulose, copper fiber powder, graphene composite material, polyvinyl alcohol powder and anti-freezing agent, stirring them for 2-3 minutes, continuously adding rosin saponification material and palm oil, stirring for 2-3 minutes.