• 专利标题:   Modified graphene catalytic slurry comprises solvent, dispersant, binder, additive and modified graphene.
  • 专利号:   CN110327908-A
  • 发明人:   JIANG H, HU J, LI J, QI C
  • 专利权人:   DAYING JUNENG TECHNOLOGY DEV CO LTD
  • 国际专利分类:   B01J020/20, B01J020/28, B01J020/30, B01J021/18, B01J031/06, B01J035/02, B01J035/10, C02F001/00, C02F001/28, C02F101/10, C02F101/16
  • 专利详细信息:   CN110327908-A 15 Oct 2019 B01J-021/18 201988 Pages: 16 Chinese
  • 申请详细信息:   CN110327908-A CN10618555 10 Jul 2019
  • 优先权号:   CN10618555

▎ 摘  要

NOVELTY - A modified graphene catalytic slurry comprises 4000-90000 pts. wt. solvent, 20-200 pts. wt. dispersant, 500-3000 pts. wt. binder, 0-1000 pts. wt. additive and 1000-3000 pts. wt. modified graphene. The solvent is water, dimethylformamide, N-methylpyrrolidone and dimethylacetamide. The dispersant is polyvinylpyrrolidone, sodium dodecylsulfonate and polyvinyl alcohol. The binder is sodium carboxymethylcellulose, hydroxypropylmethylcellulose, polytetrafluoroethylene, polyvinylidene fluoride, polyvinyl alcohol and styrene-butadiene rubber. The additive is adsorbed carbon material with BET specific surface area of 1200 m2/g. The modified graphene is rich in edge, pore structure, five-membered ring, seven-membered ring and hetero atom. USE - A modified graphene catalytic slurry. ADVANTAGE - The product is low-cost, has viscosity of 3500-6500 mPa Pa.s, has simple preparation, has high catalytic activity, suitable for water body treatment, energy efficient and environment-friendly. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of modified graphene catalytic slurry comprising: (A) utilizing water as solvent, dividing binder iinto first binder and second binder; first binder comprises sodium carboxymethyl cellulose or hydroxypropyl methylcellulose; and second binder comprises polytetrafluoroethylene, polyvinylidene fluoride, polyvinyl alcohol and styrene-butadiene rubber, mixing 70000-90000 pts. wt. water, 150-250 pts. wt. first binder and 20-100 pts. wt. dispersant, stirring to obtain first intermediate product, mixing with 2500-3000 pts. wt. modified graphene, stirring to obtain second intermediate product, and mixing and stirring with 1700-2200 pts. wt. second binder; and (B) utilizing dimethylformamide as solvent, mixing 40000-60000 pts. wt. dimethylformamide and 80-120 pts. wt. dispersant, stirring to obtain first product, mixing with 1200-1300 pts. wt. binder, stirring to obtain second product, mixing with 1300-1700 pts. wt. modified graphene, and stirring.