▎ 摘 要
NOVELTY - Preparation of carbon composite anode material comprises mixing 0.1-10 mmol organic polymer solution, 1-10 g graphene oxide solution and gas oxidant, reacting at 150-200 degrees C for 2-12 hours, carbonizing at 750-850 degrees C to obtain carbon/graphene composite, mixing carbon nanotubes, carbon source, lithium salt additive and water, adding carbon/graphene composite, mixing, solid-liquid separating, and carbonizing at 200-500 degrees C. Organic polymer is phenolic resin, epoxy resin, furfural resin, and/or acrylic resin. USE - Method for preparing carbon composite anode material. ADVANTAGE - The material has high tap density, and excellent quick charging performance.