▎ 摘 要
NOVELTY - Attapulgite-paraffin graphene composite conductive primer comprise 40-60% solvent, 25-45% thermoplastic acrylic resin, 4.5-8% conductive attapulgite, 1-6% graphite, 0.5-1% polyethylene glycol-20000, and 0.3-1% dispersant. USE - Attapulgite-paraffin graphene composite conductive primer. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of attapulgite-paraffin graphene composite conductive primer comprising mixing dispersant, polyethylene glycol-20000 and conductive attapulgite, adding graphene to solvent, stirring for 0.5-1.5 hours, adding thermoplastic acrylic resin, and mixing.