• 专利标题:   Anti-corrosion coating comprises epoxy resin, graphene/dedoped polyaniline composite, zinc, filler, colorant, dispersing agent, wetting agent, thickening agent, leveling agent, antifoaming agent, anti-bacterial agent and water.
  • 专利号:   CN105400373-A, CN105400373-B
  • 发明人:   LUO S, LI X, LIU W, YAO C, ZUO S, CAI K
  • 专利权人:   UNIV CHANGZHOU
  • 国际专利分类:   C09D163/00, C09D005/10, C09D007/12, C09D007/61
  • 专利详细信息:   CN105400373-A 16 Mar 2016 C09D-163/00 201641 Pages: 12 English
  • 申请详细信息:   CN105400373-A CN10941005 16 Dec 2015
  • 优先权号:   CN10941005

▎ 摘  要

NOVELTY - Anti-corrosion coating comprises 20-80 wt.% epoxy resin, 5-15 wt.% graphene/dedoped polyaniline composite, 5-10 wt.% zinc, 5-10 wt.% filler, 1-10 wt.% colorant, 0.1-3 wt.% dispersing agent, 0.1-3 wt.% wetting agent, 0.1-3 wt.% thickening agent, 0.1-1 wt.% leveling agent, 0.1-1 wt.% antifoaming agent, 0.1-1 wt.% anti-bacterial agent and 1-35 wt.% water. USE - Used as anti-corrosion coating. ADVANTAGE - The coating: has increased dispersion and no agglomeration. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is also included for preparing the anti-corrosion coating comprising weighing graphene/dedoping polyaniline composite, zinc, epoxy resin, filler, dispersing agent, wetting agent, defoaming agent, thickening agent and anti-bacterial agent, stirring for 20-30 minutes, adding water, mixing well, adding colorant and leveling agents and stirring to obtain anti-corrosion coating.