▎ 摘 要
NOVELTY - Anti-corrosion composite material comprises 40-60 pts. wt. glass fiber, 30-45 pts. wt. polyvinyl chloride (PVC), 5-12 pts. wt. aluminum hydroxide, 35-50 pts. wt. Teflon (RTM: PTFE), 2 pts. wt. redispersible powder, 2-5 pts. wt. stabilizer, 2-8 pts. wt. foaming agent, 1-3 pts. wt. graphene, 10-15 pts. wt. polypropylene, 1-4 pts. wt. antioxidant and 3 pts. wt. composite modified diatomite. USE - Anti-corrosion composite material. ADVANTAGE - The material reduces production cost, has light weight, good insulating property, anti-pollution property, excellent corrosion resistance and easy molding and manufacturing performance and is stable. DETAILED DESCRIPTION - An INDEPENDENT CLAIM is included for preparation of the anti-corrosion composite material comprising mixing glass fiber, polyvinyl chloride, aluminum hydroxide, Teflon, redispersible powder, stabilizer, foaming agent, graphene, polypropylene and antioxidant, heating, crushing, sieving, adding composite modified diatomite, mixing, adding water, mixing, drying, melting extruding, granulating and molding.